Welcome Coastal,

I have used Quick Cast (from others called Skin and Core) some years ago, patterns built with big 3D Systems SLA, but I have not had good results, with high reactive alloy as Titanium above all.

Maybe the resin used to that time was not well developed yet, but anyway I have had bad results, now I don't know well if the used resin is the same one or if is updated.